๐ Abstract
A fiber of a propylene ethylene copolymer having:i) xylene soluble fraction at 25ยฐ C. ranging from 14 wt % to 27 wt %;ii) intrinsic viscosity of the fraction soluble in xylene at 25ยฐ C. ranging from 1.0 to 2.4 dl/g;iii) melt flow rate, MFR, ranging from 12 g/10 min to 60 g/10 min;iv) an ethylene derived units content ranging from 5.0 wt % to 12.0 wt %;v) the ethylene derived units content of the fraction insoluble in xylene at 25ยฐ C. ranging from 2.5 wt % to 6.0 wt %;vi) the ethylene derived units content of the fraction soluble in xylene at 25ยฐ C. ranging from 15.2. wt % to 30.2 wt %vii) C13 NMR sequences PEP measured on the fraction insoluble in xylene at 25ยฐ C. ranging from 3.5 mol % to 5.5 mol %; andviii) the C13 NMR sequences PEP measured on the fraction soluble in xylene at 25ยฐ C. ranging from 11.0 mol % to 14.2 mol %.