The Superalloys: Fundamentals and Applications

Roger C. Reed

📅 2008-07-31

📄 Abstract

1. Introduction 2. The physical metallurgy of nickel and its alloys 3. Single crystal superalloys for blade applications 4. Superalloys for turbine disc applications 5. Environmental degradation: the role of coatings 6. Summary and future trends.